Instruction and Application: Titanium calcium type drug skin stainless steel, 900 ~ 1100 ℃ good oxidation resistance, good welding performance, crack resistance is good. Good stomatal performance, alternating current and dc, all position welding. For welding of drum and other materials.
Typical Chemical Composition of the all-weld metal (%)
C |
Si |
Mn |
S |
P |
Cr |
Ni |
0.088 |
1.15 |
6.6 |
0.0037 |
0.019 |
23.92 |
18.60 |
Mechanical properties of all-weld metal
Temperature |
Tensile strength Rm(MPa) |
Elongation A(%) |
Bending Test (GB/T 2653) |
Room temperature |
685 |
35 |
No Cracks |
All-welded metal radio graphic testing:
According to NB/T 47013.2, the radio graphic testing should not be less than class AB and the quality grade of all-welded metal should not be less than Class I at least.
Reference Current(DC+):
Electrodes Sizeφ(mm) |
Φ2.5 |
Φ3.2 |
Φ4.0 |
Φ5.0 |
Amperage (A) |
60-90 |
90-120 |
120-160 |
170-210 |
Notice:
1.The electrode with titanium-calcium coating must be stoved at 200-300℃ for 1 hours prior to use.
2.The welding consumables surface rust, oil fouling and other impurities must be cleaned up.
3.The welding slag must be cleaned up in the multi-pass welding. The inter-pass temperature should be controlled below 150 ℃.